MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Tygon® S3™ B-44-4X Phthalate-free Food, Milk, and Dairy tubing
Categories: Polymer; Thermoplastic

Material Notes: Tygon S3™ B-44-4X, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-based Tygon S3™ line combines the high performance standards customers demand with an eco-friendly tubing design.

Tygon S3™ Food, Milk and Dairy Tubing offers dependable performance in countless filling, draining, transfer and processing applications. Its smooth, non-porous bore inhibits particle entrapment, promoting a sanitary fluid path by minimizing potential for bacterial growth. It has outstanding resistance to harsh alkaline cleaners and is equally unaffected by commonly used sanitizers.

Non-toxic, taste-free and odor-free, Tygon S3™ Food, Milk and Dairy Tubing meets applicable regulatory standards for contact with food products. Complete clarity for positive visual inspection and flow control, it is available in up to a 6" inside diameter, making it a flexible replacement for rigid piping systems.

Applications

  • Aseptic filling
  • Condiment dispensing
  • Dairy processing
  • Soft-serve dispensing
  • Vitamin and flavor concentrate systems

Features and Benefits

  • Smooth, non-porous bore will not trap particulates or promote bacterial growth
  • Compatible with foods containing a high oil content
  • Resistant to harsh alkaline cleaners and sanitizers
  • Excellent alternative to rigid piping systems
  • Contains no BPA or phthalates

Regulatory Information: Tygon S3™ complies with FDA, NSF, 3-A, Japan Food Sanitation Law # 370/1959, REACH, 1935/2004/EC and 10/2011/EC for many foods and beverages. Tygon S3™ tubing products do not contain chemicals listed in California's Prop 65.

Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM placques or molded ASTM durometer buttons.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Water Absorption 0.22 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 66
@Time 15.0 sec
ASTM D2240
Tensile Strength 2200 psiASTM D412
Tensile Stress at Strain 1379 psi
@Strain 200 %
Elongation at Break 390 %ASTM D412
Tear Strength 250 pliASTM D1004
Compression Set 59 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395 Method B
Tensile Set 57 %at 75% Elongation; ASTM D412-98
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Minimum Service Temperature, Air -49.0 °Ctemperature limit for flexibility
Brittleness Temperature -32.0 °FASTM D746
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Clear, but value not quantified
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA Yes
NSF Yes
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation
Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation
Saint-Gobain Tygon® Noroprene® Chemical Tubing Formulation
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture

PSTGQ913 / 160409

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.