MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® K222-KMV5 /A PA6-MD25 FR(30)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: 25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccdry; ISO 1183
Water Absorption 6.2 %Sim. To ISO 62
Moisture Absorption 1.80 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0091 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0082 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 35.0 MPacond; ISO 527-1/-2
 65.0 MPadry; ISO 527-1/-2
Elongation at Break 2.5 %dry; ISO 527-1/-2
 30 %cond; ISO 527-1/-2
Tensile Modulus 2.50 GPacond; ISO 527-1/-2
 6.00 GPadry; ISO 527-1/-2
Charpy Impact Unnotched 25.0 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eU
 29.0 kJ/m²
@Temperature 23.0 °C
dry; ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature 23.0 °C
dry; ISO 179/1eA
 2.00 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmdry; IEC 60093
Surface Resistance >= 1.00e+15 ohmcond; IEC 60093
Comparative Tracking Index 600 Vcond; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°Cdry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°Cdry; ISO 11359-1/-2
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °Cdry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °Cdry; ISO 75-1/-2
Flammability, UL94 V-2
@Thickness 1.50 mm
dry; IEC 60695-11-10
 V-2
@Thickness 0.750 mm
dry; IEC 60695-11-10
Glow Wire Ignition Temperature 700 °C
@Thickness 0.750 mm
Glow Wire Ignition Temperature, dry; IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
Glow Wire Ignition Temperature, dry; IEC 60695-2-13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® K222-KGV4 PA6-GF20 FR(30), Dry, 20% Glass Filled, Heat Stabilized, Flame Retardant
Envalior Akulon® K222-KGV5
Covestro Apec® 2095 Polycarbonate
EPICHEM Epinyl PA 66 Polyamide 66
Envalior Novamid® 1010N2 1ES NAT PA6 FR(30)

PDSM9723 / 161344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.