MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® MC2 Polyester Film, 50 Gauge (14 µm), PVDC Coated
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC) Coated Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

A polyester film with a vacuum deposited layer of aluminum on one side and overcoated on both sides with a heat sealable PVDC copolymer. The film has excellent oxygen, moisture, and light barrier properties. It is available in 50 and 100 gauge. Can be used in plain and structured form to package snacks, candy, nuts, pharmaceuticals, dry chemicals, and other materials that require protection from moisture, oxygen, and light.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Average value for Mylar® films.
Moisture Vapor Transmission 0.00800 cc-mm/m²-24hr-atm0.0203 cc-mil/100 in²-24hr-atmASTM E96 Procedure E
Water Vapor Transmission 0.600 g/m²/day0.0386 g/100 in²/dayASTM E96 Procedure E
Oxygen Transmission 0.00210 cc-mm/m²-24hr-atm0.00533 cc-mil/100 in²-24hr-atmor 0.15 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 14.0 microns0.551 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 100 %100 %ASTM D882
Film Elongation at Break, TD 80 %80 %ASTM D882
Modulus of Elasticity 3.45 GPa500 ksi(stiffness), ASTM D882
Tear Strength Test 300300Graves, g; ASTM D1004
Seal Strength 201 g/25 mm201 g/in
Film Tensile Strength at Break, MD 165 MPa23900 psiASTM D882
Film Tensile Strength at Break, TD 193 MPa28000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FNot cleared by FDA for food temperatures above this temperature.
Shrinkage 1.5 %
@Temperature 150 °C,
Time 1800 sec
1.5 %
@Temperature 302 °F,
Time 0.500 hour
Film shrinkage in oven.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® HS Polyester Film, 48 Gauge (12 µm)
DuPont Teijin Films Mylar® LBT Polyester Film, 48 Gauge (12 µm)
DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge

PDU683 / 33132

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.