MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil HTA 001HP2 High Density Polyethylene (HMW) Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughness properties as well as high stiffness.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Grocery Sacks
  • Liners
  • Refuse Bags
  • Shoppers
  • Thin Gauged Consumer Bags Information provided by ExxonMobil
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D4883
Melt Flow 9.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 5900 psiASTM D882
Film Tensile Strength at Yield, TD 4200 psiASTM D882
Film Elongation at Break, MD 210 %ASTM D882
Film Elongation at Break, TD 430 %ASTM D882
Elmendorf Tear Strength MD 7.0 gASTM D1922
Elmendorf Tear Strength TD 30 gASTM D1922
Dart Drop Test 190 gASTM D1709A
Film Tensile Strength at Break, MD 8300 psiASTM D882
Film Tensile Strength at Break, TD 7000 psiASTM D882
1% Secant Modulus, MD 170000 psiASTM D882
1% Secant Modulus, TD 170000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 259 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil HTA 001HD High Density Polyethylene (HMW) Resin
ExxonMobil HD 7960.13 HMW Blown Film Resin
ExxonMobil HPA 020 Molding High Density Polyethylene (HMW) Resin
Amco PRIMATOP HDPE HMW 1000950 High Molecular Weight Copolymer
ExxonMobil HD 5451HL High Density Polyethylene Resin

PEX99323 / 175559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.