MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical Lupox® GP2156FL PBT+GF15%  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Description: Injection Molding, PBT+GF15%, Flame Retardant

Application: IT/OA, E&E (CRT Socket)

CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.010 cm/cm
@Thickness 3.20 mm
0.0040 - 0.010 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 93.2 MPa
@Thickness 3.20 mm
13500 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 3.0 %
@Thickness 3.20 mm
3.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Yield Strength 142 MPa
@Thickness 3.20 mm
20600 psi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Flexural Modulus 4.90 GPa
@Thickness 3.20 mm
711 ksi
@Thickness 0.126 in
1.3mm/min; ASTM D790
Izod Impact, Notched 0.441 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
0.827 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D257
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
660 kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D495
Comparative Tracking Index 175 V175 VSolution A; IEC 60112
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=0.710 mm
15 - 30 sec
@Thickness >=0.0280 in
 15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
 30 - 60 sec
@Thickness >=3.30 mm
30 - 60 sec
@Thickness >=0.130 in
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.710 mm
>= 120 arcs
@Thickness 0.0280 in
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
 >= 120 arcs
@Thickness 3.30 mm
>= 120 arcs
@Thickness 0.130 in
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/min
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F@ Break; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
@Thickness 6.40 mm
401 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
@Thickness 6.40 mm
383 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical  130 °C
@Thickness >=0.710 mm
266 °F
@Thickness >=0.0280 in
 130 °C
@Thickness >=1.50 mm
266 °F
@Thickness >=0.0591 in
 130 °C
@Thickness >=3.00 mm
266 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  130 °C
@Thickness >=0.710 mm
266 °F
@Thickness >=0.0280 in
 130 °C
@Thickness >=1.50 mm
266 °F
@Thickness >=0.0591 in
 130 °C
@Thickness >=3.00 mm
266 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  130 °C
@Thickness >=0.710 mm
266 °F
@Thickness >=0.0280 in
 130 °C
@Thickness >=1.50 mm
266 °F
@Thickness >=0.0591 in
 130 °C
@Thickness >=3.00 mm
266 °F
@Thickness >=0.118 in
Flammability, UL94  V-0
@Thickness >=0.710 mm
V-0
@Thickness >=0.0280 in
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 235 - 250 °C455 - 482 °FInjection Molding
Middle Barrel Temperature 240 - 250 °C464 - 482 °FInjection Molding
Front Barrel Temperature 245 - 255 °C473 - 491 °FInjection Molding
Nozzle Temperature 245 - 255 °C473 - 491 °FInjection Molding
Melt Temperature 245 - 255 °C473 - 491 °FInjection Molding
Mold Temperature 60.0 - 100 °C140 - 212 °FInjection Molding
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hourInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupox® GP2100 PBT+GF10%
LG Chemical Lupox® GP2156FM PBT+GF15%
Iran Petrochemical (PCC) PET BG-821 Polyethylene Terephthalate
LG Chemical Lupox® HI2100M PBT+GF10%
LG Chemical Lupox® TE5100 PBT+PC+GF10%

PLAY307 / 148317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.