MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical Lupox® GP2156FL PBT+GF15%  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Description: Injection Molding, PBT+GF15%, Flame Retardant

Application: IT/OA, E&E (CRT Socket)

CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.010 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 93.2 MPa
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 3.0 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Yield Strength 1450 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus 50000 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 4.50 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
ASTM D149
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 175 VSolution A; IEC 60112
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=0.710 mm
 15 - 30 sec
@Thickness >=1.50 mm
 30 - 60 sec
@Thickness >=3.30 mm
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.710 mm
 >= 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 3.30 mm
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
 
Thermal PropertiesOriginal ValueComments
Melting Point 225 °C@ Break; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
UL RTI, Electrical 130 °C
@Thickness >=0.710 mm
 130 °C
@Thickness >=1.50 mm
 130 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 130 °C
@Thickness >=0.710 mm
 130 °C
@Thickness >=1.50 mm
 130 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 130 °C
@Thickness >=0.710 mm
 130 °C
@Thickness >=1.50 mm
 130 °C
@Thickness >=3.00 mm
Flammability, UL94 V-0
@Thickness >=0.710 mm
 V-0
@Thickness >=1.50 mm
 V-0
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 235 - 250 °CInjection Molding
Middle Barrel Temperature 240 - 250 °CInjection Molding
Front Barrel Temperature 245 - 255 °CInjection Molding
Nozzle Temperature 245 - 255 °CInjection Molding
Melt Temperature 245 - 255 °CInjection Molding
Mold Temperature 60.0 - 100 °CInjection Molding
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 - 5.00 hourInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Lupox® GP2100 PBT+GF10%
LG Chemical Lupox® GP2156FM PBT+GF15%
Iran Petrochemical (PCC) PET BG-821 Polyethylene Terephthalate
LG Chemical Lupox® HI2100M PBT+GF10%
LG Chemical Lupox® TE5100 PBT+PC+GF10%

PLAY307 / 148317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.