MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.

Available in: Asia Pacific, Europe, Latin America and North America.

Product Applications: This phosphorous flame retardant grade, UL 94 V0 (0.8 mm), offers excellent filling qualities and with good mechanical properties. This grade is suitable for molding insulating parts for electrical devices: connectors, switches, bobbins coil formers and thin parts under stress. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183/A
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPaISO 527 Type 1A
Elongation at Break 2.0 %ISO 527 Type 1A
Elongation at Yield 2.0 %ISO 527 type 1 A
Tensile Modulus 12000 MPaISO 527 Type 1A
Flexural Strength 260 MPaISO 178
Flexural Modulus 10000 MPaISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²ISO 180/1A
Charpy Impact Unnotched 65.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Strength 25.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 325 VSolution B; IEC 60112
 400 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Flammability, UL94 V-0
@Thickness 0.800 mm
ISO 1210
 V-0
@Thickness 1.60 mm
ISO 1210
Oxygen Index 30.5 %ISO 4589
Glow Wire Flammability Index 960 °CISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 275 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned
Domo TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Celanese Zytel® 70G35EF BK538 PA66-GF35
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Avient Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66)

PRHOD586 / 137817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.