MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina
Categories: Ceramic; Oxide; Aluminum Oxide; Potting/Casting Ceramic

Material Notes: Fine grain castable for potting and producing small tools.

Cure:
Step 1. Dry for 8 hours minimum at room temperature.
Step 2. Bake at 200 ºF for 2–4 hours.
Step 3. Final cure at 250 ºF for 3 hours.
Step 4. Final cure at 450 ºF for 30–60 minutes if using HLB-1 Hydrophobic Liquid Binder.

Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
Porosity <= 2.0 %<= 2.0 %
pH 2.0 - 3.02.0 - 3.0
Viscosity 11000 cP11000 cPmixed
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 81.4 MPa11800 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 ohm-cm1.00e+9 ohm-cm
Dielectric Strength 5.91 kV/mm150 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.74 µm/m-°C
@Temperature 20.0 °C
4.30 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1650 °C3000 °F
Shrinkage <= 0.30 %
@Temperature 538 °C
<= 0.30 %
@Temperature 1000 °F
 
Processing PropertiesMetricEnglishComments
Dry Time >= 8 hour>= 8 hourAir dry
Cure Time 300 - 420 min5.00 - 7.00 hour2-4 hrs at 200°F; 3 hrs at 250°F
Pot Life 60.0 - 120 min60.0 - 120 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Acid ResistanceGoodattacked by HF
Alkali ResistanceGood
BinderMgO-P2O5
ColorWhite
Mix Ratio100:13-15powder:liquid
Moisture ResistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound
Momentive Performance Materials AC6043 Titanium Diboride/Boron Nitride Composite
BryCoat WS2 Tungsten Disulfide Coating
Silver Vanadium Oxide Fluoride, Ag4V2O6F2
Corning Macor® Machinable Glass Ceramic

CAREM44 / 585

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.