MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borstar® FB4230 LLDPE for Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar FB4250T exhibits a good balance between dart impact combined with excellent yield and tensile strength and improved stiffness. Its toughness also remains in cold climate conditions. The film has good seal strength, wide sealing window and good hot tack force. In addition to the well know Borstar properties, Borstar FB4250T also give good optical properties.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccISO 1183
Water Vapor Transmission 8.00 g/m²/day
@Temperature 38.0 °C
90% RH; ISO 15106-2
Oxygen Transmission Rate 5000 cc/m²/dayAt 25°C/0% RH/1 bar; ASTM D3985
Thickness 40.0 microns
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 2.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
High Load Melt Index 40 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 %ISO 527-3
Film Elongation at Break, TD 750 %ISO 527-3
Secant Modulus, MD 0.300 GPa0.05-1.05%; ASTM D882-A
Secant Modulus, TD 0.350 GPa0.05-1.05%; ASTM D882-A
Impact 60Puncture Resistance, force (N); ASTM 5748
Puncture Energy 4.00 JASTM 5748
Elmendorf Tear Strength, MD 10.19 g/micronISO 6383/2
Elmendorf Tear Strength, TD 22.93 g/micronISO 6383/2
Dart Drop 5.00 g/micronISO 7765/1
Film Tensile Strength at Break, MD 50.0 MPaISO 527-3
Film Tensile Strength at Break, TD 40.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 124 °CISO 11357/03
Vicat Softening Point 104 °CA (10N); ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 70 %ASTM D1003
Gloss 10 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borstar® FB2230 LLDPE for Film
Borealis Borstar® FB2310 LLDPE for Film
Borealis FG5190 Linear Low Density Polyethylene
Borealis Borstar® FB4250T LLDPE for Blown Film
Borealis Borstar® FB1460 HDPE for Film

PBOREA113 / 27420

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.