MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® 7120B LLDPE Blown & Cast Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: This linear low density polyethylene is an ethylene-hexene copolymer tailored for film applications that require:
  • Excellent processing characteristics
  • Exceptional drawdown
  • Use alone or in coextrusions; blends with other polyolefins
Typical blown film applications include:
  • Coextrusions
  • Blend component to improve drawdown
  • Thin gauge applications
  • General purpose packaging Data provided by Chevron Phillips Chemical Company, LP.

    Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Thickness 31.8 microns1.25 mil
Melt Flow 2.0 g/10 min2.0 g/10 min190 °C/2.16 kg; ASTM D1238E
Slip Level 1000 ppm1000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 750 %750 %ASTM D882
Coefficient of Friction 0.700.70ASTM D1894
Elmendorf Tear Strength, MD 11.8 g/micron300 g/milNotched; ASTM D1922
Elmendorf Tear Strength, TD 29.5 g/micron750 g/milNotched; ASTM D1992
Dart Drop 5.91 g/micron150 g/milASTM D1709
Film Tensile Strength at Break, MD 44.8 MPa6500 psiASTM D882
Film Tensile Strength at Break, TD 37.9 MPa5500 psiASTM D882
1% Secant Modulus, MD 228 MPa33000 psiASTM D882
1% Secant Modulus, TD 276 MPa40000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 18 %18 %ASTM D1003
Gloss 65 %65 %60°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 °C518 °FCast Film
Die Opening 0.0640 cm0.0252 in
Extruder Size 6.35 cm2.50 in
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade
Borealis Borstar® FB2230 LLDPE for Film
Borealis FG5190 Linear Low Density Polyethylene
Borealis FG5224 Linear Low Density Polyethylene
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin

PCHEVF10 / 20271

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.