MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sibur MPP 21015-E10 Frost Resistant Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Index of Compound 1.0 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 22.0 MPa
Elongation at Break >= 200 %
Charpy Impact Unnotched >= 5.00 J/cm²
@Temperature -50.0 °C
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 130 °C10 hours at load
 
Descriptive Properties
Frost Resistance<-40°CFor painted marks
 <-50°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HC110BF Polypropylene Homopolymer
Borealis HC101BF Polypropylene Homopolymer
Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (Asia Pacific Grade)
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin (Asia Pacific Grade)

PSIB025 / 67588

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.