MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis HC101BF Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packages for bakery products, flower packaging, textile film yarns, woven fabrics, ropes and twines. HC101BF contains no slip, antiblock, antistatic additives or nucleating additives

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow  3.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.2 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 4.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
4.5 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 15 g/10 min
@Load 5.00 kg,
Temperature 230 °C
15 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 - 200 %150 - 200 %ISO 527-3
Film Elongation at Break, TD 50 - 90 %50 - 90 %ISO 527-3
Tensile Modulus 2.00 - 2.20 GPa290 - 319 ksiMD; ISO 527-2
 3.30 - 3.50 GPa479 - 508 ksiTD; ISO 527-2
Film Tensile Strength at Break, MD 130 - 160 MPa18900 - 23200 psiISO 527-3
Film Tensile Strength at Break, TD 230 - 280 MPa33400 - 40600 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 161 - 165 °C322 - 329 °FDSC; ISO 3146
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
Gloss >= 100 %>= 100 %45°C of arc; ASTM D2457
 
Descriptive Properties
Isotactic Index (Heptane Insolubles, %)96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HC110BF Polypropylene Homopolymer
Covestro Makrolon® Rx1805 Polycarbonate
Borealis HC401BF Polypropylene Homopolymer
Borealis HB205TF Polypropylene
Borealis HC207TF Polypropylene Homopolymer

PBOREA468 / 108727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.