MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis HC101BF Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packages for bakery products, flower packaging, textile film yarns, woven fabrics, ropes and twines. HC101BF contains no slip, antiblock, antistatic additives or nucleating additives

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 3.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 4.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 15 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 150 - 200 %ISO 527-3
Film Elongation at Break, TD 50 - 90 %ISO 527-3
Tensile Modulus 2000 - 2200 MPaMD; ISO 527-2
 3300 - 3500 MPaTD; ISO 527-2
Film Tensile Strength at Break, MD 130 - 160 MPaISO 527-3
Film Tensile Strength at Break, TD 230 - 280 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 161 - 165 °CDSC; ISO 3146
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Gloss >= 100 %45°C of arc; ASTM D2457
 
Descriptive Properties
Isotactic Index (Heptane Insolubles, %)96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HC110BF Polypropylene Homopolymer
Covestro Makrolon® Rx1805 Polycarbonate
Borealis HC401BF Polypropylene Homopolymer
Borealis HB205TF Polypropylene
Borealis HC207TF Polypropylene Homopolymer

PBOREA468 / 108727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.