MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexTow® IM10 Intermediate Modulus Carbon Fiber (12,000 Filaments)
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Continuous fiber can be combined with virtually all thermoset and thermoplastic resin systems. They are used for weaving, braiding, filament winding applications, unidirectional tapes for ATL and AFT processes and prepreg tow for fiber placement. The finished products have excellent corrosion, creep and fatigue resistance plus high strength and stiffness characteristics.

Information provided by Hexcel Corporation. Values are typical average lot properties.

Key Words: Carbon Fibres
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.79 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6757 MPa
Elongation at Break 2.0 %
Tensile Modulus 310 GPaat chord 6000-1000
 
Descriptive Properties
Standard Spool Size2 pounds
Weight/Length0.324 g/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexTow® HM63 High Modulus Carbon Fiber (12,000 Filaments)
Hexcel® HexTow® IMA Intermediate Modulus Carbon Fiber (12,000 Filaments)
Hexcel® HexTow® IM7 12K Intermediate Modulus Carbon Fiber (12,000 Filaments)
SGL Carbon Group SIGRAFIL C® C30 T045 EPY Continuous Tow Carbon Fiber with 45k filaments, Epoxy Sizing
Hexcel® HexTow® AS2C Carbon Fiber

EHECFCm / 230543

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.