MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; Colorable

Processing Method: Injection Molding

Forms: Pellets

Additive: Flame Retardant

Information Provided by Teknor Apex

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Linear Mold Shrinkage 0.0090 - 0.0147 in/inASTM D955
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 235 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength 10500 psiASTM D638
Elongation at Break 6.0 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Strength 14000 psiASTM D790
Flexural Modulus 455000 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Strength 380 V/mil
@Thickness 3.00 mm
ASTM D149
Comparative Tracking Index 600 VUL 746
 
Thermal PropertiesOriginal ValueComments
Melting Point 420 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 175 °FUnannealed; ASTM D648
UL RTI, Electrical 266 °F
@Thickness 0.810 mm
UL 746
 266 °F
@Thickness 1.50 mm
UL 746
 266 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 221 °F
@Thickness 0.810 mm
UL 746
 221 °F
@Thickness 1.50 mm
UL 746
 221 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 248 °F
@Thickness 0.810 mm
UL 746
 248 °F
@Thickness 1.50 mm
UL 746
 248 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.630 mm
Oxygen Index 32 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 425 - 455 °F
Middle Barrel Temperature 445 - 485 °F
Front Barrel Temperature 465 - 500 °F
Nozzle Temperature 465 - 500 °F
Melt Temperature 465 - 500 °FProcessing Temperature
Drying Temperature 175 °F
Moisture Content 0.20 %
 
Descriptive Properties
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® B 50 H1 PA66/6, DRY
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated
Domo TechnylStar™ S 60G1 V30 PA6, 30% glass filled, DRY
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant

PTEKNO417 / 128594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.