MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Solef® 32008 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.

Features: Copolymer; Good Flexibility; Low Viscosity

Uses: Wire & Cable Applications

Additional Properties: Crystallization Heat - ASTM D3417 15.0 to 22.0 J/g; Heat of Fusion - ASTM D3417 15.0 to 22.0 J/g

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 - 1.80 g/ccASTM D792
Water Absorption <= 0.040 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.020 - 0.030 cm/cm
Melt Flow 3.0 - 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47ASTM D2240
Tensile Strength at Break 14.0 - 30.0 MPa
@Thickness 2.00 mm
50 mm/min; ASTM D638
Tensile Strength, Yield 14.0 - 35.0 MPa
@Thickness 2.00 mm
50 mm/min; ASTM D638
Elongation at Break 350 - 600 %50 mm/min; ASTM D638
Elongation at Yield 10 - 12 %50 mm/min; ASTM D638
Tensile Modulus 100 - 300 MPa
@Thickness 2.00 mm
1.0 mm/min; ASTM D638
Izod Impact, Notched NB
@Thickness 4.00 mm
ASTM D256
Coefficient of Friction 0.20 - 0.40vs. Itself; ASTM D1894
Coefficient of Friction, Dynamic 0.20 - 0.30vs. Itself; ASTM D1894
Taber Abrasion, mg/1000 Cycles 5.0 - 15CS-10 Wheel, 1000 g; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohmASTM D257
Dielectric Constant 7.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 20.0 - 25.0 kV/mm
@Thickness 1.00 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 15.0 - 22.0 J/gASTM D3417
CTE, linear, Parallel to Flow 130 - 150 µm/m-°C
@Temperature 0.000 - 40.0 °C
Specific Heat Capacity 1.20 J/g-°C
@Temperature 23.0 °C
ASTM C351
 1.60 J/g-°C
@Temperature 100 °C
ASTM C351
Thermal Conductivity 0.200 W/m-K
@Temperature 23.0 °C
ASTM C177
Melting Point 165 - 170 °CDSC
Crystallization Temperature 125 - 130 °CPeak; ASTM D3418
Vicat Softening Point 75.0 °CRate A (50°C/h), Loading 2 (50 N)
Glass Transition Temp, Tg -28.0 °CASTM E1356
Oxygen Index 48 %
@Thickness 3.00 mm
ASTM D2863
 
Descriptive Properties
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
FormGranules

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Solef® 1006 Polyvinylidene Fluoride (PVDF)
Covestro Makrolon® 2400 Polycarbonate
Covestro Makrolon® 2258 Polycarbonate
Covestro Makrolon® 2256 Polycarbonate
Covestro Makrolon® 1954 Polycarbonate

PSOL8Y7292 / 177023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.