MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
Categories: Polymer; Film; Thermoplastic; Ethylene Acrylic Acid

Material Notes: 7 wt% Acrylic Acid.

Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins.

Features/Benefits: Low seal initiation temperature allows high speed packaging. Very good hot tack, seal through contamination, and heat seal strength provides strong, reliable heat seals. Balanced acid content (7% AA) provides good adhesion to both aluminum and low-density polyethylene (LDPE). In film applications, 7 melt flow index (MFI) allows for very good wetting in thermal lamination processes. In extrusion coating applications, 7 MFI provides better performance in internally deckled dies compared to higher MFI extrusion coating resins.

Typical Applications: Cable shield wrap. Sealants for sachets in both food and nonfood applications. Toothpaste tubes, as a foil/LDPE tie layer. Other foil-containing pouches and sachets. Medical/pharmaceutical packaging.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 540 %50 µm (2 mil) film; ASTM D882
Film Elongation at Break, TD 560 %50 µm (2 mil) film; ASTM D882
Secant Modulus, MD 0.170 GPa50 µm (2 mil) film; ASTM D882
Secant Modulus, TD 0.175 GPa50 µm (2 mil) film; ASTM D882
Impact 13J/mm Spencer Impact; ASTM D3420
Elmendorf Tear Strength, MD 170 g/mil50 µm (2 mil) film; ASTM D1922
Elmendorf Tear Strength, TD 160 g/mil50 µm (2 mil) film; ASTM D1922
Dart Drop Test 4.30 g
Seal Strength 2000 g/25 mmseal bar 150°C.
Film Tensile Strength at Break, MD 25.5 MPa50 µm (2 mil) film; ASTM D882
Film Tensile Strength at Break, TD 26.9 MPa50 µm (2 mil) film; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 85.0 °CFreezing Point via DSC/ASTM D3418
 102 °CUpon Melting via DSC/ASTM D3418
Vicat Softening Point 84.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 3.0 %ASTM D1003
Gloss 100 %20°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 177 °CTypical Die Temp. for blown film
Melt Temperature 160 - 175 °Cblown film equipment

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Dow Primacor® 3340 Ethylene Acrylic Acid (EAA)
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
ExxonMobil Exxtra™ Adhere EAA30010 Ethylene Acrylic Acid Copolymer Resin
BASF Lucalen® A 2710 H Ethylene/Acrylate Copolymer

PDUPJI / 33652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.