MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastics Group Polifil® BS-70 70% Barium Sulfate Reinforced Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Polifil® BS series compounds are homopolymer polypropylene resins reinforced with barium sulfate. They possess increased specific gravity, high flex modulus, high deflection temperature, good chemical resistance, frictional resistance, and x-ray opacity.

Applications:

  • Cosmetic application
  • Molded weights
  • Soundproofing components
  • Medical devices

Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/ccASTM D792
Filler Content 70 %ASTM D2584
Melt Flow 6.0 - 14 g/10 minMay be specified; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2800 psiASTM D638
Flexural Modulus 552000 psiTangent; ASTM D790
Izod Impact, Notched 0.280 ft-lb/inAt 73°F; ASTM D256
Izod Impact, Unnotched 2.78 ft-lb/inAt 73°F; ASTM D256

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman JPP50BX01BK 50% Barium Sulfate Filled, Heat-Stabilized, Homopolymer Polypropylene containing 25% P.C.R.
Techmer ES HiFill® PA6 0177 B Barium Sulfate Filler
Inno-Comp INNOPOL® CS 2-8960 60% Barium-Sulfate Filled Polypropylene Block-Copolymer
Barium Sulfate, BaSO4
Albis Plastics Polypropylene A 13 H-BS 73 , 73% Barium Sulfate Filled

PPOLI022 / 56926

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.