MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sharadaa Ceramics REFINSUL ZAP-014 Insulating Castables
Categories: Ceramic

Material Notes: Manufacturer provides a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for low density and low thermal conductivity, and are helpful in conserving heat energy thus reducing fuel costs.

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density <= 0.850 g/ccDried at 110°C
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000392 GPaDried at 110°C
 0.000294 GPa
@Treatment Temp. 1100 °C
 0.000294 GPa
@Treatment Temp. 3400 °C
Compressive Strength 4.00 kg(f)/cm²Fired at 800°C, Cold Crushing
 6.00 kg(f)/cm²Fired at Service temp. of 1100°C, Cold Crushing
 12.0 kg(f)/cm²Dried at 110°C, Cold Crushing
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.163 W/m-K
@Temperature 500 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 32 %
Fe2O3 <= 8.5 %
 
Descriptive Properties
Permanent Linear Change-1.0 - 1.0%Fired at 800°C
 -1.6 - 1.6%Fired at Service temp. 1100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sharadaa Ceramics REFCAST C High Alumina Castables
Sharadaa Ceramics Calcium Silicate Block
Thermal Ceramics K-Shield Felt AG/Min-K Composite
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized
BNZ Materials Marinite® C Ceramic Board for Aluminum Contact

CSHARA025 / 130188

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.