MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
NBE nanoTach® Nano-Silver Paste, Lead-Free Solder Alternative
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: NanoTach® is a thick paste of nano-sized silver powder in an organic binder that can be used as an alternative to solder or epoxy in semiconductor devices in the state-of-the-art individual packages or multi-chip power modules. NBE’s lead-free nanomaterial attachment possesses better thermal, mechanical and electrical properties than soldered or epoxied alternatives. The attachment process is completely compatible with existing equipment and facilities that use solders or epoxies. Using NBE’s material and process, high power-density semiconductor electronic or optoelectronic devices can be operated at high temperatures in excess of 250° C, not attainable with any existing solder-based or epoxy-based materials. Specific applications can include bonding to large chips for power devices/modules, high-power and high-brightness LED lamps, power diode lasers, and RF power devices.

Compared to the current die-attach materials, nanoTach® offers:

  • 5x higher thermal and electrical properties
  • > 250° C capability
  • < 275° C ambient or low pressure (5 MPa) processing
  • Improved reliability from low elastic modulus
  • One-to-one RoHS compliant replacements.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density >= 3.50 g/ccBefore Sintering
 >= 7.90 g/ccAfter Sintering
Solids Content >= 78.5 %Before Sintering
Porosity <= 25 %After Sintering
Viscosity 750000 cPBefore Sintering
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 10.0 - 30.0 GPaAfter Sintering
Adhesive Bond Strength >= 20.0 MPaChip Bonding
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000260 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.6 µm/m-°CAfter Sintering
Thermal Conductivity >= 2.00 W/m-K
Melting Point 961 °CAfter Sintering
Maximum Service Temperature, Air <= 961 °Cmp of silver
 
Processing PropertiesOriginal ValueComments
Sintering Temperature <= 275 °C
Shelf Life 12.0 Month
 
Descriptive Properties
ColorDark GrayBefore Sintering
RoHS CompliancyCompliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent C2100211D1 Silicone Based Silver Paste
Aremco Pyro-Duct™ 597-A Electrically & Thermally Conductive Material, Silver Filled
Atom Adhesives AA-DUCT 916 Epoxy Adhesive
Johnson Matthey Silver-flo™ 452 Cadmium Free Silver Brazing Filler Metal
Overview of materials for Copper Alloy

NNBE00 / 89271

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.