MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman HT 3380-1 Special Hardener
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Mix Ratio with GT 7013 is 18.

Comments/Applications: Acid-anhydride functional crosslinker useful in FDA powder and can coating applications. *Mix ratio with GT 7013.

Data provided by Ciba Specialty Chemicals.

Ciba Specialty Chemicals has been acquired by Huntsman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 95.0 - 110 °CSoftening Range
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 °CCure Schedule: 5/20 min @ 170/220°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman HT 2844 Special Hardener
Evonik VESTAGON® B 68 Colorant
AISI 1055 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Overview of materials for Epoxy Cure Resin
AISI 1055 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round

PCIC57 / 28556

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.