MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Master Bond MasterSil 910Med Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Key Features:
  • Meets USP Class VI requirements
  • Passes ISO 10993-5 testing
  • Very fast curing
  • Paste consistency
  • Unsurpassed performance profile
  • Excellent sterilization resistance
Product Description: MasterSil 910Med is a one part silicone for bonding, sealing and coating primarily for medical devices. It passes both USP Class VI testing and ISO cytotoxicity specifications. As an acetoxy type system, it bonds exceptionally well to a wide variety of substrates including metals, composites, ceramics, glass as well as many rubbers and plastics. MasterSil 910Med can resist the most aggressive types of thermal cycling as well as mechanical and thermal shock. Typical of one part silicones, the curing mechanism is based on the humidity level. The higher the humidity, the faster the cure and thinner sections cure more quickly than thicker ones. MasterSil 910Med is a fast curing system and depending upon the application, the tack free time can range from 10-20 minutes. It withstands liquid sterilants, gamma radiation and EtO very well. Its service temperature range is -75°F to +400°F. Most importantly One particularly useful product property is its ability to adhere well to silicone substrates. MasterSil 910Med can be used in a wide array of medical device applications where the acetoxy type cure is not an issue and optimum product properties are required. It should be emphasized that for biocompatibility testing,

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20 - 30
Tensile Strength 1300 - 1600 psi
Elongation at Break 400 - 600 %
Adhesive Bond Strength 400 - 500 psiTensile Lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 2.75
@Frequency 60 Hz
Dissipation Factor 0.0030
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -75.0 °F
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 10.0 - 20.0 min
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
Colortranslucent
Viscositypaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® R PLUS 4285/30 Solid Silicone Rubber-Batch Grade
Momentive Performance Materials Silopren™ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear
Mitsui HILET™ 2221 Porous Polyethylene Membrane
Mitsui HILET™ 1351D Porous Polyethylene Membrane
Master Bond MasterSil 153Med Silicone Paste for Medical Applications

PMASTM938 / 185531

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.