MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® NA520024 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Applications
PETROTHENE NA 520-024 is a high molecular weight, low density polyethylene resin for power, communications, coaxial and control cable insulation. An antioxidant package has been added to provide thermal stability during processing.

Processing Techniques
NA 520-024, like other thermoplastic polyolefin resins, can be processed on a conventional extruder. Suggested extrusion conditions for NA 520-024 are listed below. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size, have an effect on processing of thermoplastic resins and compounds.

This product is from the former Equistar product line.

Key Words: LDPE; Telecom/ Telecommunications; Primary Insulation
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
ESCR 10% Igepal® >= 168 hour10% Igepal; 0 failures after 168 hours; ASTM D1693
Melt Flow 0.25 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2040 psiASTM D638
Elongation at Break 570 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.29
@Frequency 100000 Hz
ASTM D1531
Dissipation Factor 0.00010
@Frequency 100000 Hz
ASTM D1531
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CF50; ASTM D746
 
Processing PropertiesOriginal ValueComments
Feed Temperature 300 - 325 °F
Zone 2 325 - 350 °F
Zone 3 350 - 375 °F
Zone 4-x 400 - 425 °F
Adapter Temperature 400 - 425 °F
Die Temperature 400 - 425 °F
Melt Temperature 400 - 425 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem H502-25RG Extrusion Polypropylene
Armacell OleTex® CKJN 1000 Polyethylene
A. Schulman CP80-01 Linear Low-Density Polyethylene
NOVA Chemicals Novapol® LE-0220-A LDPE Extrusion Resin
LyondellBasell Petrothene® NA214000 Low Density Polyethylene

PEQU0275 / 36709

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.