MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® ECO BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: PA 6, 20% glass, injection molding, halogen free flame retardant, contains at least 15% pre-consumer-recyclate

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 g/ccISO 60
Density 1.31 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0080 cm/cm60x60x2; 260 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm60x60x2; 260 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 76.0 MPa5 mm/min; ISO 527-1,-2
Elongation at Break 3.0 %5 mm/min; ISO 527-1,-2
Tensile Modulus 5400 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 140 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 135 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 5300 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 3.8 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²ISO 180-1U
Charpy Impact Unnotched 35.0 kJ/m²ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 31.9 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Comparative Tracking Index 0.00 VSolution A; UL 746A
 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 222 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °CISO 75-1,-2
Vicat Softening Point 205 °C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94 V-2
@Thickness 0.750 mm
 V-2
@Thickness 1.50 mm
 V-2
@Thickness 3.00 mm
Oxygen Index 30 %Method A; ISO 4589-2
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
Shrinkage, MD 0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD 0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
60x60x2; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °Cinjection molding
 250 - 270 °C
Mold Temperature 80.0 °Cinjection molding
 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 2.00 - 6.00 hour
Moisture Content 0.030 - 0.070 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Dry
Ensinger TECASINT™ 2021 Polyimide, Brown (PI)
Domo TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Domo TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned)

PLANW9494 / 208366

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.