MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals Electroformed Nickel, 200 Micron (8 mil) Foil, Electroformed and Annealed  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Pure Element

Material Notes: The nickel foil is made produced via a continuous electrodeposition process, producing a foil of consistent quality in greater widths and lower thicknesses than is available by conventional metal rolling, both in the hard (“as-electroformed”) and annealed conditions. Electroformed nickel foil has very high chemical purity, excellent and consistent surface finish, and good etching characteristics. Its applications include battery mesh, heating elements, bursting discs, gaskets, lead frames and printed resistor/circuit boards. Other applications utilize the inherent magnetic properties of nickel.

Available thicknesses (2019) are 8-100 microns (0.00031-0.004 in).

Data provided by the manufacturer, Special Metals.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.322 lb/in³
Thickness 8.00 mil
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 102200 g load
Tensile Strength, Ultimate 51000 psiTransverse
 52000 psiLongitudinal
Elongation at Break 28 %Transverse
 39 %Longitudinal
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000800 ohm-cm
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.010 %
Chromium, Cr <= 0.010 %
Cobalt, Co <= 0.010 %
Copper, Cu <= 0.010 %
Iron, Fe <= 0.010 %
Nickel, Ni >= 99.95 %
Sulfur, S <= 0.0020 %
Zinc, Zn <= 0.0010 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NiCoForm NiColoy® E Electroformed Nickel-Cobalt
Special Metals Electroformed Nickel, 13 Micron (0.5 mil) Foil, Electroformed and Annealed
Special Metals Electroformed Nickel Foil, As-Electroformed
Eastman Amphora™ FL6000 Flexible 3D Polymer
Celanese D Antistat 907 kg-51007157 91-93% Paraformaldehyde

NINCO81 / 17515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.