MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Glacial Acrylic Acid
Categories: Fluid; Solvent

Material Notes: Formula: C3H4O2

CAS: 79-10-7

Description: Acrylic acid glacial is a colorless liquid having a sharp, acrid odor. It is completely soluble in water. Acrylic acid is a monomer used in industrial synthesis and for producing polymers

Applications:

    Acrylic acid is a versatile a, ß-unsaturated carboxylic acid. It can enter into common reactions with a large number of organic and inorganic compounds and intermediates for the synthesis of many low and high-molecular weight compounds. Some typical reactions/applications include:
  • As a vinyl compound in addition reactions.
  • As a carboxylic acid — acrylic esters, acrylamide, N-substitute amides and acrylic acid chloride.
  • Copolymers with acrylic esters, methacrylic esters, acrylonitrite maleic acid esters, vinyl acetate, vinyl chloride, vinylidene chloride, styrene, butadiene and ethylene.
  • Homopolymers of acrylic acid and copolymers form water-soluble compounds in acid form or their alkali/ammonium salts. Uses include thickening agents; dispersing agents; protective colloids for stabilizing emulsions and polymer dispersions wetting agents. AAG is used to produce very high molecular weight polymers for flocculents and viscosity control in oil-well drilling mud.
  • Superabsorbant polymers are lightly crosslinked polyacrylic acid salts.They are used for fluid retention, largely in baby diapers, but also in products for feminine hygeine, adult incontinence and agriculture.
  • Copolymers with less than 50% acrylic acid produce polymers only slightly soluble or even insoluble in water. Their alkali or ammonium salts are used in sizes, adhesive intermediates, and binders for printing inks and coatings.
  • Copolymers with small amounts of acrylic acid improve adhesions and improve resistance to oil and solvents.
      In polymer dispersions, acrylic acid addition improves stability and compatibility with pigments.

      Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.046 g/cc0.03779 lb/in³
 1.0249 g/cc
@Temperature 30.0 °C
0.037027 lb/in³
@Temperature 86.0 °F
aqueous solutions with 25.3% acrylic acid
 1.0438 g/cc
@Temperature 30.0 °C
0.037710 lb/in³
@Temperature 86.0 °F
aqueous solutions with 50% acrylic acid
 1.0459 g/cc
@Temperature 30.0 °C
0.037786 lb/in³
@Temperature 86.0 °F
aqueous solutions with 53.5% acrylic acid
 1.0506 g/cc
@Temperature 30.0 °C
0.037955 lb/in³
@Temperature 86.0 °F
aqueous solutions with 90.4% acrylic acid
 1.0526 g/cc
@Temperature 30.0 °C
0.038028 lb/in³
@Temperature 86.0 °F
aqueous solutions with 87.7% acrylic acid
 1.0544 g/cc
@Temperature 30.0 °C
0.038093 lb/in³
@Temperature 86.0 °F
aqueous solutions with 78% acrylic acid
Solubility in Water 100 %100 %Unlimited
Viscosity  0.82 cP
@Temperature 80.0 °C
0.82 cP
@Temperature 176 °F
 0.93 cP
@Temperature 40.0 °C
0.93 cP
@Temperature 104 °F
 1.246 cP
@Temperature 30.0 °C
1.246 cP
@Temperature 86.0 °F
aqueous solutions with 25.3% acrylic acid
 1.3 cP
@Temperature 20.0 °C
1.3 cP
@Temperature 68.0 °F
 1.715 cP
@Temperature 30.0 °C
1.715 cP
@Temperature 86.0 °F
aqueous solutions with 50% acrylic acid
 1.785 cP
@Temperature 30.0 °C
1.785 cP
@Temperature 86.0 °F
aqueous solutions with 53.5% acrylic acid
 1.835 cP
@Temperature 30.0 °C
1.835 cP
@Temperature 86.0 °F
aqueous solutions with 90.4% acrylic acid
 1.973 cP
@Temperature 30.0 °C
1.973 cP
@Temperature 86.0 °F
aqueous solutions with 87.7% acrylic acid
 2.092 cP
@Temperature 30.0 °C
2.092 cP
@Temperature 86.0 °F
aqueous solutions with 78% acrylic acid
Vapor Pressure  0.000900 bar
@Temperature 0.000 °C
0.675 torr
@Temperature 32.0 °F
 0.00380 bar
@Temperature 20.0 °C
2.85 torr
@Temperature 68.0 °F
 0.0135 bar
@Temperature 40.0 °C
10.1 torr
@Temperature 104 °F
 0.0399 bar
@Temperature 60.0 °C
29.9 torr
@Temperature 140 °F
 0.238 bar
@Temperature 100 °C
179 torr
@Temperature 212 °F
 0.500 bar
@Temperature 120 °C
375 torr
@Temperature 248 °F
 1.00 bar
@Temperature 141 °C
750 torr
@Temperature 286 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.93 J/g-°C0.461 BTU/lb-°F
Melting Point 13.0 °C55.4 °FFreezing Point
Boiling Point 141 °C286 °F
Flash Point 54.0 °C129 °F
Ignition Temperature 390 °C734 °FAutoignition
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.42 - 1.4211.42 - 1.421
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.070 %<= 0.070 %ED-070
 
Descriptive Properties
Assay>99.7%ED-049
Color<10ED-071
CompositionDimer, by HPLC500 ppm, ED-083
 Inhibitor content180-220 ppm, ED-073
Dissociation Constant5.74E-05
Heat of Combustion19085 kJ/kg
Heat of Neutralization806 kJ/kg
Heat of Polymerization1079 kJ/kg
Latent Heat of Evaporation at Boiling Point634 kJ/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF N-Butanol
BASF Butyl Acrylate
BASF 2-Ethylhexanol
Evonik TEGO® Antifoam 2280 Emulsion
Evonik TEGO® Antifoam PVC 100 Organomodified siloxane

PBASG0858 / 132491

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.