MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Alpase K100-S™ Aluminum Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: K100-S™ features and benefits include: Dimensional stability, fully weldable, anodizable, high elongation, consistent properties - regardless of size, close flatness and tolerances, superior corrosion resistance, can be nickel plated, smoothest aluminum surface finish.

Applications:Can be painted on both sides, including heat-cured finishes; used for mold cooling and heating plates without impregnation; low pressure molds for shoes, skis, etc.; plate for composite tooling requiring vacuum integrity and dimensional stability.

Sizes: Thickness 0.25 -8 inches; Width 38.25, 48.5, and 60.5 inches (custom up to 88 inches); Length 96.5 and - 144.5 inches. Data provided by Alpase.

Key Words: Aluminium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0960 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 70
Tensile Strength, Ultimate 283 MPaTypical
Tensile Strength, Yield 124 MPaTypical
Elongation at Break 12 - 15 %Typical
Modulus of Elasticity 71.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000590 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.8 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 117 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 94 %as balance
Copper, Cu 0.10 - 0.20 %
Iron, Fe 0.10 - 0.40 %
Magnesium, Mg 4.0 - 4.9 %
Manganese, Mn 0.40 - 1.0 %
Silicon, Si 0.00 - 0.40 %
Zinc, Zn 0.00 - 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alpase K100™ Aluminum Plate
Alcoa 7055-T7751 Aluminum Plate
Alcoa MIC-6 Aluminum Mold Alloy
Alcoa 2324-T39 Aluminum Plate
Alclad Aluminum 6061-T6, T651

NALPASE0 / 14949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.