MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hostaform® S 9364 POM, Impact Modified
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Hostaform« acetal copolymer grade S 9364 is highly impact modified grade for demanding applications. Hostaform« S 9364 provides a significant improvement in impact strength and flexibility over standard impact modified grades such as Hostaform« S 9063 and S 9064.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183
Water Absorption at Saturation 0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.016 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cmISO 294-4
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
[cm3/10min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 43.0 MPa50mm/min; ISO 527-2/1A
Elongation at Yield 16 %50mm/min; ISO 527-2/1A
Tensile Modulus 1650 MPa50mm/min; ISO 527-2/1A
Flexural Modulus 1550 MPaISO 178
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 21.0 kJ/m²ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-2
Melting Point 166 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 140 °CISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 70.0 °Ccavity
Zone 1 170 - 180 °C
Zone 2 180 - 190 °C
Zone 3 180 - 190 °C
Zone 4 180 - 200 °C
Die Temperature 180 - 200 °C
Melt Temperature 180 - 200 °C
Drying Temperature 80.0 - 100 °C
Dry Time 3.00 hour
Injection Pressure 60.0 - 120 MPa
Hold Pressure 60.0 - 120 MPa
Back Pressure <= 2.00 MPa
 
Descriptive Properties
Injection moldingYes
Injection speedslow
Processing conditions acc. ISO9988-2
Profile extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hostaform® S 9364 WS 10/1570 POM, UV Resistant
Celanese Hostaform® S 9243 XAP2 ™ POM, Impact Modified
Celanese Hostaform® S 9362 POM, Impact Modified
Celanese Hostaform® S 9364LPB POM, Impact Modified
Celanese VECTRA A725 LCP, 25% Specialty

PHCQ423 / 178878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.