MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Devcon Magic Bond™ Epoxy Putty
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Emergency Repair Products

Comments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded, machined, tapped or drilled when fully cured. Waterproof formula cures well under water and remains sealed long-term. Mixes quickly, hardens in 30-40 minutes. For plumbing repairs and marine use.

Data provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0654 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength, Ultimate 2450 psiASTM D638
Tensile Modulus 700 ksiASTM D638
Flexural Yield Strength 4280 psiASTM D790
Compressive Yield Strength 12000 psiASTM D695
Adhesive Bond Strength 700 psiAdhesive tensile shear strength; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 28.1ASTM D150
Dielectric Strength 300 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.00124 cal cm/sec-cm²-°CASTM C177
Maximum Service Temperature, Air 250 °FOperating Temperature
Shrinkage 0.30 %During Cure; ASTM D2566
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 °F
Pot Life 20.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Coverage per lb.61 in²at 1/4 inch thick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, sublimed
Silicon Carbide, CVD
Silicon Carbide, Alpha SiC
Silver, Ag
Silicon Nitride

PITWX17 / 48504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.