MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.64 g/cc1.64 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 103 MPa14900 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 6.89 GPa999 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 165 MPa23900 psi1.3 mm/min; ASTM D790
Flexural Modulus 6.89 GPa999 ksi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.800 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.50 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Coefficient of Friction, Dynamic 0.570.57vs. Steel - Dynamic; ASTM D1894
Coefficient of Friction, Static 0.410.41vs. Steel; ASTM D1894
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
@Thickness 6.35 mm
421 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Descriptive Properties
FeaturesGood Chemical Resistance
 High Heat Resistance
 High Rigidity
 Lubricated
 Semi Crystalline
FormsPellets
Generic MaterialPBT
Generic NamePolybutylene Terephthalate (PBT)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAppliance Components
 Automotive Applications
 Bearings
 Business Equipment
 Consumer Applications
 Conveyor Parts
 Gears
 Industrial Applications
 Printer Parts
 Pulleys
 Rollers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
Avient LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66)
Avient LubriOne™ PC-1000 Polycarbonate
Aluminum Titanium Nitride (AlTiN) PVD Coating
3M GM641 Soft Gripping Material

PH0POL1341 / 145910

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.