MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nitriflex NitriClean 3355 NBR - Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General use for technical artifacts that require resistance to oils and greases with good processability and low mold fouling.

Applications: Rings, gaskets, joints.

Information provided by Dax Resinas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.00 - 0.70 %0.00 - 0.70 %Method B-003; ASTM D5668
Mooney Viscosity 45 - 55
@Temperature 100 °C
45 - 55
@Temperature 212 °F
ML1+4, Method B-002; ASTM D1646
Ash 0.00 - 1.0 %0.00 - 1.0 %ASTM D5667
 
Descriptive Properties
AppearanceWhite to yellowish
Bound Acrylonitrile Content (%)31 - 34ASTM D3533
PolymerizationCold

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
ATG s.r.l. NBR Nitrile-Butadiene Rubber
KKPC KOSYN KNB 35LL Acrylonitrile Butadiene Rubber (NBR)
Versalis Europrene® N 3345 GRN Acrylonitrile-Butadiene Rubber
Nitriflex N-726 NBR - Nitrile Rubber

PDAX043 / 29468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.