MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® eXten D 437P PA6.10, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced material. This material is available in natural.

Benefits: This polyamide 6,10 for extrusion is specially performing where high flexibility and toughness are requested. It is specially developed for automotive and other applications where a long term high temperature usage is requested.

Key Properties: Translucency; UV stabilized; High impact at low temperature and High flexibility

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC This grade complies with RoHS directive 2002/95/EC Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: Extrusion pipes and tubing applications.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183/A
Water Absorption 1.9 %1.9 %ISO 62
 0.65 %
@Time 86400 sec
0.65 %
@Time 24.0 hour
ISO 62
Viscosity  700 cP
@Shear Rate 1000 1/s,
Temperature 230 °C
700 cP
@Shear Rate 1000 1/s,
Temperature 446 °F
 1000 cP
@Shear Rate 100 1/s,
Temperature 230 °C
1000 cP
@Shear Rate 100 1/s,
Temperature 446 °F
 5000 cP
@Shear Rate 10 1/s,
Temperature 230 °C
5000 cP
@Shear Rate 10 1/s,
Temperature 446 °F
Linear Mold Shrinkage, Flow 0.022 cm/cm0.022 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0241 cm/cm0.0241 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868ISO 868
Tensile Strength at Break 44.0 MPa6380 psiISO 527 Type 1A
Tensile Strength, Yield 40.0 MPa5800 psiISO 527 Type 1A
Tensile Stress at Strain  12.0 MPa
@Strain 20 %,
Temperature 150 °C
1740 psi
@Strain 20 %,
Temperature 302 °F
 12.0 MPa
@Strain 100 %,
Temperature 150 °C
1740 psi
@Strain 100 %,
Temperature 302 °F
 15.0 MPa
@Strain 20 %,
Temperature 135 °C
2180 psi
@Strain 20 %,
Temperature 275 °F
 15.0 MPa
@Strain 160 %,
Temperature 150 °C
2180 psi
@Strain 160 %,
Temperature 302 °F
 16.0 MPa
@Strain 100 %,
Temperature 135 °C
2320 psi
@Strain 100 %,
Temperature 275 °F
 20.0 MPa
@Strain 160 %,
Temperature 135 °C
2900 psi
@Strain 160 %,
Temperature 275 °F
 23.0 MPa
@Strain 20 %,
Temperature 80.0 °C
3340 psi
@Strain 20 %,
Temperature 176 °F
 27.0 MPa
@Strain 100 %,
Temperature 80.0 °C
3920 psi
@Strain 100 %,
Temperature 176 °F
 30.0 MPa
@Strain 160 %,
Temperature 80.0 °C
4350 psi
@Strain 160 %,
Temperature 176 °F
 40.0 MPa
@Strain 20 %,
Temperature 23.0 °C
5800 psi
@Strain 20 %,
Temperature 73.4 °F
 41.0 MPa
@Strain 100 %,
Temperature 23.0 °C
5950 psi
@Strain 100 %,
Temperature 73.4 °F
 43.0 MPa
@Strain 160 %,
Temperature 23.0 °C
6240 psi
@Strain 160 %,
Temperature 73.4 °F
Elongation at Break <= 200 %<= 200 %ISO 527 Type 1A
Tensile Modulus 0.820 GPa119 ksiISO 527 Type 1A
Flexural Modulus 0.720 GPa104 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 215 - 220 °C419 - 428 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C126 °FISO 75/Af
 
Processing PropertiesMetricEnglishComments
Feed Temperature 200 - 220 °C392 - 428 °F
Front Barrel Temperature 215 - 235 °C419 - 455 °F
Die Temperature 210 - 230 °C410 - 446 °F
Drying Temperature 80.0 °C
@Time 28800 sec
176 °F
@Time 8.00 hour
dew point -35°C
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Compression Zone210-230°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® eXten D 437P PA6.10, Conditioned
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Multibase TPSiV® 4200-80A Thermoplastic Silicone Vulcanizate
BASF Ultramid® 8253 HS PA6 (Conditioned)

PRHOD556 / 137787

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.