MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® eXten D 437P PA6.10, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced material. This material is available in natural.

Benefits: This polyamide 6,10 for extrusion is specially performing where high flexibility and toughness are requested. It is specially developed for automotive and other applications where a long term high temperature usage is requested.

Key Properties: Translucency; UV stabilized; High impact at low temperature and High flexibility

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC This grade complies with RoHS directive 2002/95/EC Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: Extrusion pipes and tubing applications.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183/A
Water Absorption 1.9 %ISO 62
 0.65 %
@Time 86400 sec
ISO 62
Viscosity 700 cP
@Shear Rate 1000 1/s,
Temperature 230 °C
 1000 cP
@Shear Rate 100 1/s,
Temperature 230 °C
 5000 cP
@Shear Rate 10 1/s,
Temperature 230 °C
Linear Mold Shrinkage, Flow 0.022 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0241 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ISO 868
Tensile Strength at Break 44.0 MPaISO 527 Type 1A
Tensile Strength, Yield 40.0 MPaISO 527 Type 1A
Tensile Stress at Strain 12.0 MPa
@Strain 20 %,
Temperature 150 °C
 12.0 MPa
@Strain 100 %,
Temperature 150 °C
 15.0 MPa
@Strain 20 %,
Temperature 135 °C
 15.0 MPa
@Strain 160 %,
Temperature 150 °C
 16.0 MPa
@Strain 100 %,
Temperature 135 °C
 20.0 MPa
@Strain 160 %,
Temperature 135 °C
 23.0 MPa
@Strain 20 %,
Temperature 80.0 °C
 27.0 MPa
@Strain 100 %,
Temperature 80.0 °C
 30.0 MPa
@Strain 160 %,
Temperature 80.0 °C
 40.0 MPa
@Strain 20 %,
Temperature 23.0 °C
 41.0 MPa
@Strain 100 %,
Temperature 23.0 °C
 43.0 MPa
@Strain 160 %,
Temperature 23.0 °C
Elongation at Break <= 200 %ISO 527 Type 1A
Tensile Modulus 820 MPaISO 527 Type 1A
Flexural Modulus 720 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 14.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 215 - 220 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Feed Temperature 200 - 220 °C
Front Barrel Temperature 215 - 235 °C
Die Temperature 210 - 230 °C
Drying Temperature 80.0 °C
@Time 28800 sec
dew point -35°C
Moisture Content <= 0.10 %
 
Descriptive Properties
Compression Zone210-230°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® eXten D 437P PA6.10, Conditioned
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Multibase TPSiV® 4200-80A Thermoplastic Silicone Vulcanizate
BASF Ultramid® 8253 HS PA6 (Conditioned)

PRHOD556 / 137787

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.