MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott S7000 Plassive Glasses Laser Cavity Material
Categories: Ceramic; Glass; Optical

Material Notes: S7000 is a clear, cerium-doped silicate glass used as a laser cavity material. It is also available to serve as a UV cut-off material. S7005 is a laser cavity material with 5 % doping of samarium oxide. This material is usually thicker than 6 mm. S7010N is a laser cavity material with 10 % doping of samarium oxide. This glass is recommended for most applications. SCHOTT offers a complete line of commercial filter glasses and can produce with a full range of doping levels for specific applications.

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.83 g/cc0.102 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 1.21.2pH=0.3 at 25°C
Alkali Class, AR 1.01.0pH=12 at 25°C
Stain Resistance Class, FR 1.01.0pH=4.6, 100 h at 25
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 78.0 GPa11300 ksi
Poissons Ratio 0.2470.247
Shear Modulus 31.3 GPa4540 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.1 µm/m-°C
@Temperature 20.0 - 300 °C
6.17 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity  0.800 W/m-K
@Temperature 25.0 °C
5.55 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
 0.960 W/m-K
@Temperature 90.0 °C
6.66 BTU-in/hr-ft²-°F
@Temperature 194 °F
Transformation Temperature, Tg 452 °C846 °F
Softening Point 598 °C1110 °F107.6
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.552
@Wavelength 1054 nm
1.552
@Wavelength 1054 nm
 1.561
@Wavelength 1054 nm
1.561
@Wavelength 1054 nm
 1.563
@Wavelength 587.6 nm
1.563
@Wavelength 587.6 nm
nd
Transmission, Visible 55.7 %55.7 %
UV Transmittance 10 %
@Wavelength 300 nm
10 %
@Wavelength 300 nm
 
Descriptive Properties
Climatic resistance1-2Water Vapor at 40-50°C for 30 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSGT9920 / 183173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.