MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott S7000 Plassive Glasses Laser Cavity Material
Categories: Ceramic; Glass; Optical

Material Notes: S7000 is a clear, cerium-doped silicate glass used as a laser cavity material. It is also available to serve as a UV cut-off material. S7005 is a laser cavity material with 5 % doping of samarium oxide. This material is usually thicker than 6 mm. S7010N is a laser cavity material with 10 % doping of samarium oxide. This glass is recommended for most applications. SCHOTT offers a complete line of commercial filter glasses and can produce with a full range of doping levels for specific applications.

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.83 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 1.2pH=0.3 at 25°C
Alkali Class, AR 1.0pH=12 at 25°C
Stain Resistance Class, FR 1.0pH=4.6, 100 h at 25
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 78.0 GPa
Poissons Ratio 0.247
Shear Modulus 31.3 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.1 µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity 0.800 W/m-K
@Temperature 25.0 °C
 0.960 W/m-K
@Temperature 90.0 °C
Transformation Temperature, Tg 452 °C
Softening Point 598 °C107.6
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.552
@Wavelength 1054 nm
 1.561
@Wavelength 1054 nm
 1.563
@Wavelength 587.6 nm
nd
Transmission, Visible 55.7 %
UV Transmittance 10 %
@Wavelength 300 nm
 
Descriptive Properties
Climatic resistance1-2Water Vapor at 40-50°C for 30 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSGT9920 / 183173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.