MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Corning 1.9 / 31 Blanc Very high Index glass
Categories: Ceramic; Glass; Optical

Material Notes: Application : Ophthalmic lenses : single vision, Progressive addition

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.99 g/cc
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.50 µm/m-°C
Softening Point 750 °C
Annealing Point 650 °C
Strain Point 750 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.87654
@Wavelength 656.3 nm
Line: C; Hydrogen
 1.87785
@Wavelength 643.8 nm
Line: C'; Cadmium
 1.8850
@Wavelength 587.6 nm
Line: d; Helium
 1.89178
@Wavelength 546.1 nm
Line: e; Mercury
 1.90543
@Wavelength 486.1 nm
Line: F; Hydrogen
 1.90742
@Wavelength 480 nm
Line: F'; Cadmium
Abbe Number 30.4ve
 30.6vd
Transmission, Visible 81 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
Blue light transmission factor
 82.6 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
Luminous; ISO 8980-3
UV Transmittance <= 0.10 %
@Thickness 2.00 mm
Solar UV-B transmission factor
 17 %
@Thickness 2.00 mm
Solar UV-A transmission factor
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
 25 %
@Wavelength 315 - 380 nm,
Thickness 2.00 mm
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott GM35429 Dental Glass
Borosilicate Glass
Advanced Ceramics ACL 2089 Cordierite
Accuratus MACOR Machinable Glass Ceramic
Plexiglas® Spelling Note

CCORN908 / 233319

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.