MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Murtfeldt Murinyl® Polyvinylidinefluoride
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposure to UV radiation. This material is ideally suited for use in the food sector and medical industry.

Special Properties:
• Good wear resistance
• Good rigidity
• High compressive strength
• High constant service temperature
• Good resistance to chemicals
• Resistant to sterilization
• No stress corrosion possible
• Very good resistance to UV rays and adverse weather conditions
• No moisture absorption
• Approved for use in the food industry (EU and FDA)

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PVDF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.79 g/cc0.0647 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.010 %
@Temperature 23.0 °C
0.010 %
@Temperature 73.4 °F
50% RH
Water Absorption at Saturation 0.050 %
@Temperature 23.0 °C
0.050 %
@Temperature 73.4 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878DIN 53505
Tensile Strength, Yield 50.0 MPa7250 psiISO 527-1/-2
Creep Strength 10.0 MPa1450 psistress leading to 1% elongation; ISO 899-1
Modulus of Elasticity 2.30 GPa334 ksi
Compressive Yield Strength  17.0 MPa
@Strain 1 %
2470 psi
@Strain 1 %
dry; ISO 604
 32.0 MPa
@Strain 2 %
4640 psi
@Strain 2 %
dry; ISO 604
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.350.35
Sand Slurry 2121µm/km
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  6.0
@Frequency 1e+6 Hz
6.0
@Frequency 1e+6 Hz
IEC 60250
 7.4
@Frequency 100 Hz
7.4
@Frequency 100 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1
Dielectric Loss Index  0.025
@Frequency 100 Hz
0.025
@Frequency 100 Hz
IEC 60250
 0.165
@Frequency 1e+6 Hz
0.165
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear  125 µm/m-°C
@Temperature 23.0 - 60.0 °C
69.4 µin/in-°F
@Temperature 73.4 - 140 °F
 140 µm/m-°C
@Temperature 23.0 - 100 °C
77.8 µin/in-°F
@Temperature 73.4 - 212 °F
Melting Point 175 °C347 °FISO 11357-1
Maximum Service Temperature, Air  150 °C
@Time 7.20e+7 sec
302 °F
@Time 20000 hour
 160 °C
@Time <=86400 sec
320 °F
@Time <=24.0 hour
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flammability, UL94 V-0V-0
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Manifattura Cattaneo PVDF
Quantum PVDF
CENTROPLAST CENTROFLON Polyvinylidene fluoride
Omnia Plastica Kynar® PVDF
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber

PMURT933 / 156580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.