MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Delrin Delrin® 500TL NC010 POM-SD
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes: Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Water Absorption 0.90 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.170 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.017 cm/cmISO 294-4, 2577
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
cm³/10min Volumetric; ISO 1133
 14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 71.0 MPaISO 527-1/-2
Elongation at Break 20 %Nominal; ISO 527-1/-2
Elongation at Yield 13 %ISO 527-1/-2
Tensile Modulus 3300 MPaISO 527-1/-2
Flexural Modulus 3100 MPaISO 178
Poissons Ratio 0.37
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -40.0 °C
ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 160 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 170 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 5.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 62631-3-1
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.6
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 165 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 103 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 3.00 mm
IEC 60695-11-10
Flame Spread 63.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 215 °COptimum, Injection
 210 - 220 °CRange, Injection
Mold Temperature 90.0 °COptimum, Injection
 80.0 - 100 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 80.0 - 100 MPaInjection
 100 MPaInjection
Annealing Temperature 160 °COptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.3Injection
Part Marking Code>POM-SD<ISO 11469
PolymerPOM-Z
Processing Hold Pressure Time (s/mm)8Injection
Resin IdentificationPOM-SDISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 100STE NC010 POM-HI
DuPont Mobility and Materials Delrin® 500TE NC010 POM-I
Delrin Delrin® 500T BK602 POM-I
Delrin Delrin® 500AF POM-SF20
Delrin Delrin® 500T NC010 POM-I

PDSX5126 / 197766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.