MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Bapolene 222B is a butene linear low density polyethylene for blown film applications requiring superior impact strength and toughness. It complies with US FDA 21CFR177.1520.

Applications: Bags; Film; Industrial Applications; Liners; Packaging.

Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers

Key Words: Butene Comonomer; Food Contact Acceptable; Good Toughness; High Impact Resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D-1505
Melt Flow 2.0 g/10 minASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 600 %ASTM D-882
Film Elongation at Break, TD 700 %ASTM D-882
Elmendorf Tear Strength MD 110 gASTM D-1922
Elmendorf Tear Strength TD 350 gASTM D-1922
Dart Drop Test 75.0 gASTM D-1709
Film Tensile Strength at Break, MD 26.9 MPaASTM D-882
Film Tensile Strength at Break, TD 18.9 MPaASTM D-882
1% Secant Modulus, MD 25000 psiASTM D-882
1% Secant Modulus, TD 27500 psiASTM D-882
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
processFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borstar® FB2230 LLDPE for Film
Borealis FG5190 Linear Low Density Polyethylene
Borealis FG5224 Linear Low Density Polyethylene
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin
A. Schulman CP814-01 Linear, Low-Density Polyethylene

PBP1118 / 83165

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.