MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 246SI V11 PA6, 11% glass filled, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Description: Polyamide 6, reinforced with 11% of glass fiber, with high impact resistance, for injection molding.

Available in: Asia Pacific

Product Applications: TECHNYL® C 246SI V11 has good mechanical properties and impact strength at low temperature. This grade is widely used for: ski boot parts. This product is available in natural color and colors in request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa13100 psiASTM D638
Elongation at Break 7.0 %7.0 %ASTM D638
Flexural Strength 135 MPa19600 psiASTM D790
Flexural Modulus 4.10 GPa595 ksiASTM D790
Izod Impact, Notched 1.95 J/cm3.65 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Feed Temperature 250 - 280 °C482 - 536 °F
Front Barrel Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone250-280°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Domo TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY
Domo TECHNYL® C 52G1 V20 GREY R7035 PA 6 20% Glass Reinforced, Conditioned
Domo TECHNYL® C 218 V50 BLACK PA 6 50% Glass Reinforced, Conditioned
Domo TECHNYL® C 216 V30 Black Z/4 PA 6 30% Glass Reinforced, Conditioned

PRHOD807 / 138038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.