MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil EXACT™ 8203 Octene-1 Plastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene based octene plastomer produced in a solution polymerization process using a metallocene catalyst. Designed for applications requiring high flexibility, outstanding toughness, excellent low temperature flex-cracking resistance and high clarity. This material combines favorable melt strength with an excellent processability, offering important advantages for foam, wire and cable and extrusion applications. Suitable for improving the impact resistance or flexibility of molded polyolefins.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.882 g/ccISO 1183
Mooney Viscosity 9.5
@Temperature 125 °C
ML (1 + 4); ASTM D1646
Environmental Stress Crack Resistance >= 1000 hourASTM D1693
Thickness 1.575 mil
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8515s; ISO 868
Hardness, Shore D 2815s; ISO 868
Tensile Strength at Break 3191 psiISO 527-2
Elongation at Break 2000 %
Flexural Modulus 4061 psiISO 178
Izod Impact, Notched NBASTM D256
 NB
@Temperature -40.0 °C
ASTM D256
Impact 100Puncture resistance max. tension, MPa; Internal Method
 1200Puncture Resistance Energy, MJ/mm; Internal Method
Dart Drop >= 406.4 g/milASTM D4272
1% Secant Modulus, MD 3480 psiASTM D882
1% Secant Modulus, TD 3480 psiASTM D882
Heat Seal Strength Initiation Temperature 64.0 °CInternal Method
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 100 J/gDSC; ASTM D3418
Melting Point 161.6 °FDSC peak melting point; ASTM D3418
Vicat Softening Point 123.8 °Fat 10 N; ISO 306
Brittleness Temperature <= -103 °FASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 2.4 %ASTM D1003
Gloss 83 %ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 8203 Plastomer for Polymer Modification
ExxonMobil EXACT™ 8201 Plastomer for Polymer Modification
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Dow ATTANE™ 4201G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer

PEXB355 / 37660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.