MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMW® 28 Copper Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: CMW® 28 material is a copper base alloy having very high electrical and thermal conductivity and medium strength and toughness. It is a heat treatable alloy and develops its strength and hardness through a combination of heat treatment and cold working. In more massive sections it will have reduced strength and hardness. CMW® 28 material is supplied in rod form.

CMW® 28 material is used very successfully in the form of resistance welding electrodes. It is recommended for the welding of coated steel and materials of high conductivity excluding silver and copper. CMW® 28 material has a machinability rating of 20 with free cutting brass being 100.

Information provided by CMW Inc.

1

Key Words: UNS C15000 (Wrought)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.89 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 70
@Diameter <=15.9 mm
Rod
Tensile Strength, Ultimate 455 MPa
@Diameter <=15.9 mm
Rod
Tensile Strength, Yield 386 MPa
@Diameter <=15.9 mm
Rod
Elongation at Break 10 %
@Diameter <=15.9 mm
Rod
Modulus of Elasticity 130 GPaBar, Rod & Strip
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000192 ohm-cmBar & Rod (90% IACS)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.3 µm/m-°C
@Temperature 100 °C
Thermal Conductivity 367 W/m-K
Melting Point 980 - 1080 °C
Solidus 980 °C
Liquidus 1080 °C
Softening Point 500 °CPermanent Softening
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 99.85 %
Zirconium, Zr 0.15 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMW® 328 Copper Alloy
CMW® 3 Copper Alloy
96Sn-4Ag Tin-Silver Solder, ASTM Class 96TS, ISO/DIS 9453 Alloy 28
AISI 1045 Steel, cold drawn, low temperature, stress relieved round (16 - 22 mm)
Cadi 150 Copper Alloy

NCMW067 / 15879

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.