MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotchkote™ EG 513 Epoxy Ceramic Rebuild
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Ceramic Repair EG 513 has been specifically developed as a ceramic filled repair system for rebuilding and repairing equipment requiring good mechanical strength, combined with abrasion and erosion resistance

Product Features:

  • Designed for application by trowel or spatula
  • Designed for use to repair cracked pump housings, worn impellers, propellers, guide vanes, valves, and tube sheets
  • Excellent adhesion to correctly prepared metal surfaces

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Thickness <= 12.0 mil
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 10000 psi
Compressive Strength 15000 psi
Shear Strength 2500 psiTensile Shear Adhesion
Abrasion 0.060[g] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 90.0 °Cpost cured 24 hrs at 100°C
 
Processing PropertiesOriginal ValueComments
Cure Time 120 hourFull Cure
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1301/GF/30/TF/15 PPS, linear with glass fiber and PTFE
Chesterton ARC 982 100% Novolac acid resistant coating
Chesterton ARC 855 Abrasion Control Coating
Prodways PLASTCure Pattern 2500 Liquid Resin for 3D Printing
Prodways PLASTCure ABS 3650 3D Printing Polymer

PMM35294 / 170041

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.