MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® L 20H FWA black 9225 PA12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded parts, and is in particular suitable for parts with low to medium wall thicknesses. This material allows further the molding of thick articles with walls up to 15 mm.
  • high impact strength
  • high elongation at break
  • very low moisture absorption
  • good chemical resistance
  • easy processing
  • low density
The particular stabilization package of Grilamid L 20 H FWA black 9225 allows the use in direct contact with potable water and foodstuff.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccDry; ISO 1183
Water Absorption 1.5 %Sim. to ISO 62
Moisture Absorption 0.700 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
@Time 15.0 sec
Conditioned; ISO 868
Tensile Strength, Yield 40.0 MPaConditioned; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 12 %Conditioned; ISO 527-1/-2
Tensile Modulus 1100 MPaConditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 100 °CLong Term; ISO 2578
 150 °CShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Compliance PropertiesOriginal ValueComments
FDA YesMedical
 
Descriptive Properties
Food contactEU Requirements
 NSF 51
FormGranules
Industry & Consumer goodsHeating systems
 Housewares
 Sanitary, water and gas supply
ProcessingInjection Molding
Product AttributesHydrolysis resistant
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)
Water ContactACS
 DVGW W270
 KTW
 NSF 61
 WRAS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsamid® AESN BLACK P202 T6L PA12-I
EMS-Grivory Grilamid® L 20 HL black 9563 PA12
Arkema Rilsamid® AECV BLACK T8L PA12
EMS-Grivory Grilamid® L 25H FWA black 9225 PA12
EMS-Grivory Grilamid® L 16 W 20 black 9995 PA12

PGRH037 / 156746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.