MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled; Thermoplastic Polyimide, Molded, PTFE Filled

Material Notes: TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.
    Main Features
  • High thermal and mechanical capacity
  • Good radiation-resistance
  • Low outgassing
  • Easily machined to tight tolerances
  • Flame retardant according to UL94 V-0
  • Very creep resistant
  • Good sliding properties
  • Broad chemical compatibility
  • Sensitive to hydrolysis in higher thermal range

    Applications
  • Mechanical engineering
  • Materials handling equipment
  • Aircraft and aerospace industries
  • Precision engineering
  • Automotive industry
  • Nuclear and vacuum technology
  • Textile industry

Preferred Fields

Valve seating, switch parts, chain guides, piston rings, guide piece, thrust washer, bearings

Information Provided by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.48 g/cc
@Temperature 23.0 °C
DIN 53 479
Filler Content 10 %PTFE
 15 %Graphite
Water Absorption at Saturation 2.3 %
@Temperature 80.0 °C
3 week saturation; EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
@Temperature 23.0 °C
DIN 53 505
Tensile Strength, Yield 77.0 MPa
@Temperature 23.0 °C
EN ISO 527
Elongation at Break 2.9 %
@Temperature 23.0 °C
EN ISO 527
Flexural Strength 120 MPa
@Temperature 23.0 °C
EN ISO 178
Flexural Strain at Yield 3.6 %EN ISO 178
Compressive Yield Strength 227 MPa10% Strain; EN ISO 604
Compressive Strength 227 MPa
@Temperature 23.0 °C
EN ISO 604
Izod Impact, Notched (ISO) 27.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 51.0 µm/m-°C
@Temperature 50.0 - 200 °C
DIN 53 752
Glass Transition Temp, Tg 330 °CDMTA
Flammability, UL94 V-0
 
Descriptive Properties
ColorBlack Gleamy
DIN-AbbreviationPI CS15 TF10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)
Ensinger TECASINT 1611 Polyimide, 30% PTFE Filled (PI)
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
Ensinger TECASINT™ 2062 Polyimide, Anthrazit Gleamy, 15% Graphite, 10% PTFE (PI)
Ensinger TECASINT 1011 Polyimide (PI)

PENSIN048 / 98109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.