MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Boron, B
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
a Lattice Constant 4.91 Å
c Lattice Constant 12.6 Å
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 10.8111995
Atomic Number 5
X-ray Absorption Edge 66.289 ÅK
Electronegativity 2.04Pauling
Ionic Radius 0.230 ÅCrystal Ionic Radius for Valence +3
 0.350 ÅCrystal Ionic Radius for Valence +1
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 3300
Hardness, Mohs 9.5
Tensile Strength, Ultimate 1.60 - 2.40 MPaAmorphous
 2.60 - 3.10 MPaCrystalline
Tensile Modulus 0.440 GPa
Compressive Strength <= 0.500 MPaB2O3 inclusions
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00200 ohm-cm
@Temperature 600 °C
 0.0120 ohm-cm
@Temperature 520 °C
 0.0400 ohm-cm
@Temperature 320 °C
 30.0 ohm-cm
@Temperature 170 °C
 400 ohm-cm
@Temperature 100 °C
 6500 ohm-cm
@Temperature 25.0 °C
 30000 ohm-cm
@Temperature 0.000 °C
 40000 ohm-cm
@Temperature -10.0 °C
 400000 ohm-cm
@Temperature -150 °C
Magnetic Susceptibility -6.20e-7cgs/g
Band Gap 1.55 eV
Electron Mobility, cm²/V-s 10
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 2050 J/g
Heat of Vaporization 3140 J/g
CTE, linear 8.20 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.0297 J/g-°C
@Temperature -191 - -78.0 °C
 0.754 J/g-°C
@Temperature -76.0 - 0.000 °C
 1.285 J/g-°C
@Temperature 0.000 - 100 °C
 1.62 J/g-°C
@Temperature 100 °C
 1.976 J/g-°C
@Temperature 500 °C
 2.135 J/g-°C
@Temperature 900 °C
Thermal Conductivity 27.4 W/m-K
Melting Point 2300 °C
Boiling Point 4000 °C
Heat of Formation 397.1 kJ/mol
Debye Temperature 1097 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 3.40
 
Component Elements PropertiesOriginal ValueComments
Boron, B 100 %
 
Descriptive Properties
CAS Number7440-42-8

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum, Al
Silver, Ag
Gold, Au
Americium, Am
Chromium, Cr; Recrystallized

AMEB000 / 8

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.