MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Petromont 4100 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petromont HDPE 4100 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for general use in large diameter heavy duty and non pressure pipe applications. The applications include profile and corrugated pipes, sewers, culverts and communication conduits.

Petromont HDPE 4100 is a high molecular weight hexene modified resin with a broad molecular weight distribution offering excellent extrusion characteristics and processability, combined with an excellent toughness and excellent stress cracking resistance. This grade’s material classification is PE345440A according to the standard ASTM D 3350-02a, according to D 3350-05, it became PE445440A. It is not a pressure rated resin.

Key Words: Non pressure pipe, corrugated pipe
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D1505
ESCR 100% Igepal® >= 2000 hourF50; ASTM D1693-B
ESCR 10% Igepal® >= 1000 hourF50; ASTM D1693-B
Melt Flow 0.10 g/10 minI2; ASTM D1238
 10 g/10 minI21; ASTM D238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 34.5 MPaASTM D638
Tensile Strength, Yield 24.1 MPaASTM D638
Flexural Modulus 1.07 GPaASTM D790
Izod Impact, Notched >= 213 J/mASTM D256
 
Descriptive Properties
ProcessPipe Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Finathene® CD 522 HDPE corrugated pipe resin
Petromont 4101 High Density Polyethylene Resin
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin

PPETROM16 / 56210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.