MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Denka VINYKON S3098 PVC, S grade for refrigerator gaskets  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: A PVC resin compound offering excellent physical properties and workability. Multiple grades are available, including hard and soft, as well as those for extrusion and injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccJIS-Z-8807
Evaporation Loss 0.30 %JIS-A-5756
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70JIS-K-6301
Tensile Strength at Break 15.21 MPaJIS-K-6723
Elongation at Break 370 %JIS-K-6723
100% Modulus 0.0063765 GPa
@Strain 100 %
JIS-A-5756
 
Thermal PropertiesOriginal ValueComments
Softening Point -24.0 °CJIS-A-5756
 
Descriptive Properties
Heating: Retention Rate of Elongation, %97JIS-A-5756
Heating: Retention Rate of Tensile Strength, %98JIS-A-5756

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ex-Tech Plastics PerformaTech™ PVC XSD-28 Static Dissipative PVC
CoreLite PVC 100 Closed-Cell PVC Foam Sheet
CoreLite PVC 48 Closed-Cell PVC Foam Sheet
Colorite Polymers CS9040UL--85B Non Lead Wire and Cable Vinyl Compound
Fainplast Compounds MPH 75/T Medical Flexible PVC, Extrusion

PDENK042 / 29706

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.