MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Advanced Ceramics MEXIM C ACL 2091
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: Mexim C has been specially formulated to give an expansion closely matched to that of copper. It has high electrical insulation properties and good mechanical strength, and finds increasing application as a conformal insulating layer on copper substrates as well as conventional electrical lead-throughs.

Information provided by Advanced Ceramics Limited (ACL)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.142 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.250 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cm
@Temperature 300 °C
 1.90e+17 ohm-cm
@Temperature 20.0 °C
Dielectric Constant 5.8
@Frequency 10000 Hz
 5.8
@Frequency 1e+8 Hz
 6.2
@Frequency 3.00e+9 Hz
Dielectric Strength 28.0 kV/mmBreakdown
Dissipation Factor 0.00020
@Frequency 1e+8 Hz
 0.00085
@Frequency 10000 Hz
 0.00265
@Frequency 3.00e+9 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 - 17.7 µm/m-°C
@Temperature 20.0 - 700 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Advanced Ceramics ACL 2089 Cordierite
96% Silica Consolidated Reconstructed Glass
Borosilicate Glass
Accuratus MACOR Machinable Glass Ceramic
Advanced Ceramics ACL 2088 Zinc Alumino-Silicate

CADVC07 / 471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.