MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit® 0192/0193 Conductive Silicone Sealant/Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Comments: Rec. bond line thickness: < 0.4 mm; flexible past.

Typical Applications: Bonding Ag/Cu elastomer gaskets; thin bond gap.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.80 g/cc
Volatile Organic Compounds (VOC) Content 0.00 g/l
Thickness 254 microns
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 1.38 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.040 ohm-cm
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 24.0 °C
Shelf Life 9.00 Month
 
Descriptive Properties
FillerAg/Cu
Resin SystemSilicone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QSil 440 Condensation Cure Silicone Adhesive
CHT Group QGel 311 QSI Quantum Silicones General Purpose Silicone Gel
CHT Group AS1802 (1084G) SILCOTHERM 1 Part RTV silicone adhesive
Chemical Concepts Chem-Set™ RTV5818 Silicone adhesive sealant
Bostik Pure Silicone 100% Silicone Sealant

PCHOME416 / 131126

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.